Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K2203-0278 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K2203-0143 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K2203-1545 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K9-0096 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K3-106 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K9-0084 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K9-0094 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K3-12 |
filingDate |
2007-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ef4999edd20864c3aa3de1efe2865744 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2c4137322d6e474adaf79704f9470af5 |
publicationDate |
2008-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2008251417-A |
titleOfInvention |
Conductive film and manufacturing method thereof |
abstract |
In the production of a conductive film effective for shielding electromagnetic waves, the surface resistance of a film after development is reduced. A method for producing a conductive film includes a metal silver forming step of forming a metal silver portion by exposing and developing a photosensitive material having a silver salt-containing layer containing a silver salt on a support; A smoothing process for smoothing the metallic silver part. And the said smoothing process is performed by a calendar roll. In this case, the smoothing process using the calendar roll is performed at a linear pressure of 1960 N / cm (200 kgf / cm) or more. [Selection] Figure 2 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2010143665-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010199052-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8017306-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011131500-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009125855-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009125854-A1 |
priorityDate |
2007-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |