Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bfe885803ddfc021f4f5ad13b5cc26b5 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-303 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-3028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-302 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-3016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-3062 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-3012 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-306 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-3008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-3038 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-3036 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-3044 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L22-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C49-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C49-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B1-02 |
filingDate |
2005-10-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e60bcb6b1e9e94e952f333f6495785b5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fb13951e2d7b3f102c4956262d984577 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1ac131b43cb50974f41c88aa31f4226a |
publicationDate |
2007-04-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2007099360-A |
titleOfInvention |
Multilayer polyester container and method for producing the same |
abstract |
To provide a multilayer polyester container excellent in functions such as transparency and barrier performance even when a functional resin or a functional resin composition having a large stretching stress is used as an intermediate layer. In a multilayer polyester container comprising inner and outer layers made of a polyester resin and at least one intermediate layer made of a functional resin, the polyester inner layer is measured at 80 ° C. in dynamic viscoelasticity (DMS) measurement at 0.5 Hz. And a difference in tan δ at 60 ° C. is 0.035 or less. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9095997-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016531774-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2123425-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2010035654-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5652204-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019072995-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008117474-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2335923-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011235569-A |
priorityDate |
2005-10-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |