Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bfe885803ddfc021f4f5ad13b5cc26b5 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L22-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C43-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-88 |
filingDate |
2003-12-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e60bcb6b1e9e94e952f333f6495785b5 |
publicationDate |
2005-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2005171081-A |
titleOfInvention |
Polyester resin for compression molding and preform and polyester container made of this resin |
abstract |
PROBLEM TO BE SOLVED: To provide a polyester resin for compression molding in which the drawdown tendency at the time of melt extrusion is effectively suppressed and the production efficiency can be improved. A polyester resin for compression molding, comprising a polyester resin containing 0.01 to 0.3 mol% of a polyfunctional component and having a melt tension of 40 mN or more. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2007123240-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8293162-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007099360-A |
priorityDate |
2003-12-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |