Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B9-06 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B9-12 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-55 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-04 |
filingDate |
2005-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4764ac804990c94b7afa2d9ef215e826 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_57df0b19f56d89543f5b37414637b41e |
publicationDate |
2007-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2007063428-A |
titleOfInvention |
Ethylene-vinyl alcohol copolymer resin composition and method for producing the same |
abstract |
PROBLEM TO BE SOLVED: To provide a resin composition excellent in barrier properties, excellent in melt moldability and local deterioration resistance. Moreover, the manufacturing method of the novel EVOH resin composition which does not necessarily need to immerse a hydrous EVOH resin composition on an acidic condition, and can reduce an acidic component is provided. [MEANS FOR SOLVING PROBLEMS] An ethylene-vinyl alcohol copolymer resin composition containing at least one kind of metal ions (A), wherein metal ions (A1) extracted by immersion treatment in hot water are converted into metal elements. An ethylene-vinyl alcohol copolymer having a metal ion (A2) of 1.0-10 mol / g or less and extracted by immersion in a 0.01 N hydrochloric acid aqueous solution in terms of metal element Let it be a resin composition. Moreover, after bringing the ethylene-vinyl alcohol copolymer resin composition having a moisture content of 10 to 80% by weight into contact with water (E1) containing metal ions (A), it is brought into contact with pure water (E2). It is set as the manufacturing method of the ethylene-vinyl alcohol copolymer resin composition characterized by these. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9073293-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011118648-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014111793-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2011118648-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021166276-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5933852-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2015174396-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5619874-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009084509-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8765037-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009084510-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2021134230-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10053566-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7356404-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015174396-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010289172-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018131543-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9221194-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014177644-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2599297-C2 |
priorityDate |
2005-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |