abstract |
PROBLEM TO BE SOLVED: To provide a thermoplastic resin composition having little metal corrosivity and excellent thermal conductivity. SOLUTION: Thermoplastic resin (component A) 99 to 20 parts by weight, apparent density is 0.15 g / cm 3 or less, and pH of aqueous layer is 4 to 10 when 5 g of graphite powder is dispersed in 100 g of water. A thermoplastic resin composition comprising 1 to 80 parts by weight of graphite (component B), preferably graphite (component B) having a particle thickness of 5 μm or less and a particle diameter of 0.1 to 500 μm . [Selection figure] None |