abstract |
The present invention provides a polyamide resin composition comprising a semi-aromatic polyamide (A) having a melting point of 280-320° C., an aliphatic polyamide (B), and 5-30 mass % of a phosphinic acid metal salt (C) , 5 to 60 mass % of reinforcing material (D), 0.1 to 8 mass % of metal carbonate (E), and 0.01 to 3 mass % of fatty acid barium salt (F), the total content of (A) and (B) It is 30-85 mass %, and the mass ratio (A/B) of (A) and (B) is 90/10-40/60. |