http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007021931-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4ad033f38114362cc6d607044dbc8ff9 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 |
filingDate | 2005-07-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ea91ba8816836b15f95cf6eebbf62e70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d27905063987aace7335494e3309c60b |
publicationDate | 2007-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2007021931-A |
titleOfInvention | Release film |
abstract | PROBLEM TO BE SOLVED: To provide a release film of the present invention not only for optical applications such as LCD, PDP, organic electroluminescence and the like for production of display members, but also for applications that extremely dislike the presence of oligomer-derived foreign matter on the film surface. It can be preferably used. A release film having a release layer on one side of a polyester film stretched at least in a uniaxial direction substantially free of an antimony element, and the content of oligomer derived from polyester in the polyester film is 0.7. For protecting the pressure-sensitive adhesive layer, wherein the amount of oligomer extracted from the surface of the release layer of the release film by dimethylformamide after heat treatment at 180 ° C. for 10 minutes is 1.5 mg / m 2 or less. Release film. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011224904-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011231262-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015202656-A |
priorityDate | 2005-07-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 48.