http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006281458-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2786295e61d306bf527292c8aea9ff7a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K1-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-08 |
filingDate | 2005-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a11468a52c3f7e986bdcaa46f996ce08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d793b0dc28c5ca60955bf8256c42911f |
publicationDate | 2006-10-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006281458-A |
titleOfInvention | Double-sided metal plate |
abstract | PROBLEM TO BE SOLVED: To provide a double-sided metal plate which is excellent in heat resistance such as bonding property and solder heat resistance and workability, and has good dimensional stability and folding resistance required for a double-sided metal plate. The present invention is a double-sided metal plate 10 in which a heat-resistant resin layer 12 adjacent to an outermost metal layer 13 is provided on at least one surface of a three-dimensional cross-linked resin layer 11, and the heat-resistant The double-sided metal plate 10 is characterized in that the glass transition temperature of the resin layer 12 is 260 ° C. or higher and the tensile elongation is 10% or higher. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5441686-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008147439-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008016603-A |
priorityDate | 2005-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 27.