http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006069808-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a55946e0f4dc12baad5eb7062ac05c7f |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B16-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B28B1-52 |
filingDate | 2004-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a71f066b0448015ff74c65e9d68d53f8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a94a36da6c395cc4398e1b6320e0e717 |
publicationDate | 2006-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006069808-A |
titleOfInvention | Inorganic board and method for producing the same |
abstract | An object of the present invention is to provide an inorganic plate having high strength and greatly improved dimensional stability and freeze-thaw resistance. [MEANS FOR SOLVING PROBLEMS] A water-soluble resin is added to a raw material mixture mainly composed of a cement-based inorganic material, a siliceous material, and a wood reinforcing material to further improve strength and improve dimensional stability and freeze-thaw resistance. In the case of manufacturing an inorganic board by adding and dispersing the raw material mixture in water to form a raw material slurry to form a paper mat, pressing the paper mat and curing it at a temperature of 150 ° C. or higher, By setting the mass ratio of the inorganic inorganic material and the siliceous material to be in the range of 35:65 to 45:55, the curing reaction of the inorganic plate is promoted to reduce the amount of unreacted substances, and thus the water-soluble resin. Eliminates the problem of delayed cement hardening. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015067488-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111763055-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008100877-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006169001-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012153574-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006169000-A |
priorityDate | 2004-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 54.