filingDate | 2003-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4c3fc0dde1e4e45d93c39879e80c6026 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_13fa8d798611fab5b9a73e467e063729 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_be0be52eb1816c3bb7f475d9203f8510 |
publicationDate | 2005-04-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005107099-A |
titleOfInvention | Method for producing sequential biaxially stretched retardation film and uniaxially stretched cast film used therefor |
abstract | An object of the present invention is to provide excellent display quality such as contrast in a wide field of view in the front and perspective directions, with little retardation and optical axis variation in the plane of a retardation film formed from polycarbonate. The invention also provides a method for producing a retardation film that can be directly bonded to a polarizing plate capable of forming a liquid crystal display device for obtaining a uniform display in a plane that does not cause spotted light on a black display screen. . SOLUTION: A step of forming polycarbonate into a cast film by a solution cast film forming method, a longitudinal stretching step of stretching the cast film in the casting direction, and a transverse stretching step of stretching in a direction orthogonal to the casting direction. The in-plane film thickness variation of the uniaxially stretched uniaxially stretched cast film stretched in the longitudinal (or lateral) stretching process is 5 μm or less, and the uniaxial The uniaxially stretched cast film containing 0.1 to 1.0% by weight of the solvent in the stretched cast film is stretched in a direction substantially perpendicular to the stretching direction. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10632696-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9709701-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016139104-A |
priorityDate | 2003-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 85.