abstract |
(57) [Problem] To provide a toner excellent in low-temperature fixability and excellent in high-temperature offset resistance. SOLUTION: This is a toner obtained by polymerizing a polymerizable monomer composition comprising at least a polymerizable monomer, a colorant, a polar resin, an ester wax, and a crosslinking agent represented by the following formula. 135 ℃ ・ 68.6N (load 7k The melt index (MI) value in g) is 10 to 100 g / 10 min. Embedded image [In the formula, R 1 represents a hydrogen atom or an alkyl group having 1 to 3 carbon atoms, R 2 represents a linear or branched alkylene group having 2 to 6 carbon atoms, and n represents 0 to 20. ] |