Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d9cb217f83556ce2a418344c2d485415 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2377-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-12569 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31681 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K1-0346 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K3-381 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-021 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-34 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K1-03 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C14-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C14-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-088 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K3-38 |
filingDate |
2001-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e23598053bd89274426200c3840a69a0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d19272329614987d2a66ca4601a24c6b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_738b9c9495230dfdea7a4ee4819b30e0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7a426a5a2bed30320892b3b030712c17 |
publicationDate |
2002-10-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2002293965-A |
titleOfInvention |
Surface treatment method and polyimide film having metal thin film |
abstract |
PROBLEM TO BE SOLVED: To provide a polyimide film having a small decrease in peel strength even after a metal thin film laminated polyimide film having a metal thin film formed on the surface of a biphenyltetracarboxylic acid-based polyimide film is placed under heating or humidifying conditions. And a polyimide film having a metal thin film. SOLUTION: The surface of a polyimide film having a biphenyltetracarboxylic acid component is treated with a solution containing potassium permanganate and / or sodium permanganate and potassium hydroxide and / or sodium hydroxide, followed by acid treatment. Surface treatment method to improve adhesion to metal by using |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2010074056-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20160111960-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10149394-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006270020-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5346040-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010144179-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007320195-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4692096-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2005004050-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012045745-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2006129526-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101269816-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2004050352-A1 |
priorityDate |
2001-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |