Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7acd9416af412b5972feb55a5e652ea2 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K1-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K21-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D161-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K3-46 |
filingDate |
2001-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4ad8e1c9986790af9030984f38ffddbb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f410dc53371e9e91ac9b91751000c3a5 |
publicationDate |
2002-09-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2002249552-A |
titleOfInvention |
Phosphorus-containing epoxy resin composition, resin sheet, metal foil with resin, prepreg, laminated board, multilayer board |
abstract |
PROBLEM TO BE SOLVED: To provide a phosphorus-containing epoxy resin composition having high flame retardancy and heat resistance without containing halogen and having excellent adhesiveness. The present invention relates to a phosphorus-containing epoxy resin composition containing a phosphorus-containing epoxy resin and a curing agent as essential components. As a phosphorus-containing epoxy resin, a phosphorus-containing organic compound obtained by reacting an organic phosphorus compound having one active hydrogen bonded to a phosphorus atom in a range of 1.01 mol or more and less than 2 mol per 1 mol of a quinone compound And the following formulas (1) to (3) Is selected from the epoxy resins represented by the following formulas (1) to (3) in an amount of 20 to 45% by mass in the total amount of the phosphorus-containing epoxy resin. Use what has been reacted so that it is contained. A part or all of a triazine-modified novolak resin is used as a curing agent. Embedded image |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006222409-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010235872-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009214525-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007507588-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007291227-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102515192-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10716728-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009074036-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10307990-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2017313809-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2010109948-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7037314-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20190035509-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I410441-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002249540-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019059845-A |
priorityDate |
2001-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |