http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002062054-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6241ba07e1a1c778c602f7915fb350f0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B6-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F27D11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F27B14-06 |
filingDate | 2000-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8b06671794f6509546f20a4c1fa23598 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5aa8a051d68a55c159356535fe19e1b2 |
publicationDate | 2002-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002062054-A |
titleOfInvention | Induction heating melting furnace |
abstract | (57) [Summary] [PROBLEMS] To obtain a molten metal with high dissolution efficiency. SOLUTION: A side wall portion 9 formed by arranging a plurality of conductive segments 8 in a circumferential direction mutually insulated from each other. And a furnace main body 1 for accommodating the metal to be melted 20 at a temperature lower than the reaction temperature so as to be coolable, and induction heating arranged on the outer peripheral side of the side wall portion 9 for inductively heating the metal to be melted 20 accommodated in the furnace main body And a coil 11. The furnace body 1 has a thermal conductivity that is lower than the reaction temperature and lowers the cooling capacity, The entire structure is made of a metal material such as chromium copper having a thermal conductivity smaller than that of pure copper. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009046339-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2014058175-A1 |
priorityDate | 2000-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 206.