http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000133987-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fec576c38e34882531ca37d6b922bf42 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K9-00 |
filingDate | 1998-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8b2e10183879bfd002d875ce23bcb50f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3409302a160e2421ca897ca046be7bdf |
publicationDate | 2000-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000133987-A |
titleOfInvention | Glass with conductive film |
abstract | (57) [Problem] To provide a vitreous thick film so that even a single plate can be used without deteriorating or deteriorating a conductive film (metal film). UV blocking, Glass with a conductive film with coloring and other functions. SOLUTION: In a glass with a conductive film in which a plurality of thin film layers including a metal film are formed on at least one surface of a glass plate, and a metal compound film is disposed on the outermost layer, a low film thickness of 2 μm or more is further formed on the surface. Glass with a conductive film formed by applying a glassy thick film made of melting point glass. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008102822-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002271086-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012219007-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009022736-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4668438-B2 |
priorityDate | 1998-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 24.