http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-19839080-B4
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_84eea7fbd30ce53cdf446437f612b20c |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2327-06 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-12 |
filingDate | 1998-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2004-06-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4bd07465de58700a093693e9f2e8536f |
publicationDate | 2004-06-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | DE-19839080-B4 |
titleOfInvention | Process for the production of gel-like PVC molding compounds with rubber-elastic properties and use of the process products |
abstract | Process for the production of gel-like PVC molding compounds with rubber-elastic properties and a Shore hardness A according to DIN 53505 of less than 20, characterized in that a dry mixture of 100 parts by weight of a vinyl chloride polymer produced by the suspension polymerization process with a K value according to DIN 53726 of at least 95 and 10 to 250 parts by weight of plasticizer are produced and then melted at a temperature of 80 ° C to 250 ° C and so much plasticizer is mixed in this temperature range that the amount of plasticizer is at least 251 parts by weight of plasticizer per 100 parts by weight of vinyl chloride polymer. |