Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fb0d40cfa9e7a08b87532d8f9c74dffd |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01R33-28 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01R33-28 |
filingDate |
1995-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cc6d9dafd32d6b8b3fa291cc48e25dc4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_51519cdcea7a14762a4eca8f4c6af7b6 |
publicationDate |
1997-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
DE-19531117-A1 |
titleOfInvention |
MRI-compatible material (titanium alloy) |
abstract |
The material is of exceptional hardness and suitable for nuclear spin. It is etched with a wet chemical etching, etching the material of the processing tool. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-19725891-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-19808220-B4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7087077-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-0061203-A1 |
priorityDate |
1995-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |