Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a6af1d249d3467c1f7c221c31f11e429 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_545bfa165f00d138c5d6ebabac1c3cdc |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M2101-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2201-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M2200-25 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M13-473 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D02G3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M14-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M10-025 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M101-06 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M14-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M10-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-473 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G3-04 |
filingDate |
2021-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d57d0f26c8cfdaa7ebf8636eb047c3b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3b18440b00a0c1c059c010dc178f2ebc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ff18e8ec9994c4d9e940d29691c77886 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_64f4eda8fe6a7162265b91a6b9acb0af http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f1b5a3d97d23db935c563efc283571ff |
publicationDate |
2022-01-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-113897714-A |
titleOfInvention |
A kind of lyocell/cotton fiber blended yarn and preparation method thereof |
abstract |
The invention relates to the technical field of home textiles, in particular to a lyocell/cotton fiber blended yarn and a preparation method thereof. The preparation method includes the following steps: S1. Cotton fiber modification treatment: soak the cotton fiber in a swelling agent, wash and dry it, treat it with helium plasma, and place it in glycidyl methacrylate under an oxygen-isolated environment The modified cotton fiber is obtained by reacting in the alcoholic solution of , and then washed and dried to obtain the modified cotton fiber; S2. The lyocell fiber and the modified cotton fiber are respectively combed and mixed, and then spun to obtain the blended yarn. Through the above grafting reaction, the ester group that is difficult to be oxidized is grafted to the cotton fiber, which solves the problem that the cotton fiber is oxidized in the air for a long time to generate carbon dioxide and water, and the intramolecular hydrogen bond is weakened and the mechanical properties are degraded. . The textile made from the blended yarn of the present invention has soft hand feeling and good comfort. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115341315-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115341315-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115075008-A |
priorityDate |
2021-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |