http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105802607-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2211-188 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07F7-003 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07F7-24 |
filingDate | 2016-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105802607-B |
titleOfInvention | A kind of MAPbX3The preparation method of perovskite nano-cluster |
abstract | A kind of MAPbX of the present invention 3 The preparation method of perovskite nano-cluster, belongs to the technical field of semiconductor nano material preparation.Halogenation methylamine solution is added to N 2 In the halogenation lead solution of protection, reacted 1 minute at a temperature of 0~25 DEG C, that is, obtain MAPbX 3 Perovskite nano-cluster.Nano-cluster prepared by the present invention has very sharp symmetrical absorption and fluorescence peak, show good luminosity and fluorescence quantum efficiency, whole operation is simple, mild condition, and can largely it synthesize, point suffers from huge application prospect in fields such as biological fluorescent labelling, light emitting diode and solar cells. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109256475-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109256475-A |