Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_25a2aa0672f345d0cc7d40e711b89003 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C1-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C1-026 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C1-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C1-02 |
filingDate |
1998-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aab562cc0a5fed830ddda46ab8673f8a |
publicationDate |
1999-04-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-9920805-A1 |
titleOfInvention |
Molten aluminum treatment |
abstract |
A method of grain refining aluminum, the method comprising providing a molten aluminum body (10) containing 1 to 3000 ppm titanium (13). A material (19) reactive with the titanium is introduced preferably in gaseous form to the aluminum body. The material has a component selected from the group consisting of boron, carbon, sulfur, nitrogen and phosphorus. The material and said titanium form a grain refining compound adapted for grain refining the aluminum. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112746195-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9371573-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015082947-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109811160-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112746195-B |
priorityDate |
1997-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |