Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1e70c0aeade92d7571d955d3b90ea06e |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G69-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G69-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G69-26 |
filingDate |
1997-05-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d171f010442f905765489a1e9ff7014 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ad7a255ccf51dccb6e62eb3b5f0233d9 |
publicationDate |
1997-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-9745471-A1 |
titleOfInvention |
Linear very high molecular weight polyamides and process for producing them |
abstract |
A linear polyamide having a weight average molecular weight above 200,000 is made by heating a lower molecular weight molten polyamide with thorough mixing at a temperature of about 265-300 °C for at least 5 minutes while an inert gas is swept gently through the reactor, the increase of molecular weight of the polyamide being catalyzed by a particular phosphinic acid derivative. |
priorityDate |
1996-05-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |