Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_260220c525b214105ee48ee2d77a5bf4 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-5228 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-616 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-6567 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-6565 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-6562 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3409 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2214-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-663 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2214-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-96 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-045 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C14-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-5603 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-4584 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-6269 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-571 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-624 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-62868 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B41-45 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C14-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-04 |
filingDate |
1994-05-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cca377c5ba4f4fbcaa819ed5ef0837c1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e2d4449a78724e5a57675d51df4c409f |
publicationDate |
1994-12-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-9427923-A1 |
titleOfInvention |
Silicon carboxide composite reinforced with ceramic fibers having a surface enriched in boron nitride |
abstract |
An improved fiber reinforced glass composite includes a boron-containing refractory fiber having its surface enriched with boron nitride in a matrix of a black glass ceramic having the empirical formula SiCxOy where x ranges from about 0.5 to about 2.0, preferably 0.9 to 1.6 and y ranges from about 0.5 to 3.0, preferably 0.7 to 1.8. Preferably the black glass ceramic is derived from cyclosiloxane or non-cyclic siloxane monomers containing a vinyl group attached to silicon and/or a hydride-silicon group. The boron nitride-containing fiber is the product of treating the boron-containing fiber with ammonia at a temperature between about 1125 °C and 1250 °C. Fibrous failure rather than brittle fracture under stress can be obtained. In one embodiment, composites may be oxidized in air at temperatures of up to 800 °C for 5 to 200 hours to improve the stress-strain properties. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-9641774-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5955194-A |
priorityDate |
1993-05-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |