abstract |
In the back coating containing carbon black, a nitrocellulose resin and a polyurethane resin, the present invention can improve remarkably dispersion stability with time of the coating by the use of a polyurethane resin satisfying a predetermined requirement, and can prevent the occurrence of flocculation of carbon black for more than 40 days. |