Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c7ad58d3c0b071069a8ee0cb8c8ba2e8 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2075-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2105-251 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C43-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C43-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6685 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K75-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C43-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C43-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-66 |
filingDate |
1991-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_82fca01f5a18c0bebac06cebd8b59aad http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_06e222137b6ab8eb394e6284dad2b8fa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_308d5a1c9470843ce90e4d3992b71e20 |
publicationDate |
1992-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-9210350-A1 |
titleOfInvention |
Method of producing moulded articles by compressing small particles or granules of polyisocyanate polyaddition products |
abstract |
The invention concerns the production of moulded articles by compressing small particles or granules of polyisocyanate polyaddition products in a press at pressures of up to 1,000 bar and temperatures of up to 230 C. The invention enables the strength of the moulded articles to be increased by virtue of the fact that, during compression, an additional shear stress is produced between the individual particles or granules. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-19730207-A1 |
priorityDate |
1990-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |