Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c72d118f5664072de841f9c5c34b9d99 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-485 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G65-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 |
filingDate |
1981-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b29889fb98bda9aa5fae2ba25b35863b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3add0dc271ed9d33768ba905fe567736 |
publicationDate |
1983-06-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-8302117-A1 |
titleOfInvention |
Polyphenylene ether phosphites |
abstract |
The softening points, the intrinsic viscosities and the impact resistance values of the hydroxyl-terminated thermoplastic polyphenylene ether resins are improved when these resins are "capped" (that is to say that they react). with a triaryl phosphite. The reaction takes place quickly to a useful extent during the normal time for the components to pass through an extrusion press or a molding machine. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5219951-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5071922-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5310820-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0501155-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0501155-A2 |
priorityDate |
1981-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |