Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_387abf6afc9a2cd5cfa5cd4d35f8b9fe |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-755 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-168 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-166 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-003 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-75 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-00 |
filingDate |
2022-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_61dd8237e03ca9f4ce8225faedfbcd79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9a698189e645be3f997789b719a69716 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_21f2d31aeaf4beb7259118d0476d3aa9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_58750041e519053ef8884dd019ebd961 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7ca0b843d822b7b5ec308ee74f4b70d2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0dda587ffef8ef41cbd788f2e06d6ebf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6cd446d861d007fc6227c8dff0648d4b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9c24732bf853ae61e57b9f88d2ddefa7 |
publicationDate |
2022-11-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2022228955-A1 |
titleOfInvention |
Method for the production of an isocyanate-group terminated polyoxazolidinone composition |
abstract |
The invention is related to a process for producing an isocyanate-group terminated polyoxazolidinone composition comprising the copolymerization of a polyisocyanate compound with two or more isocyanate groups with a polyepoxide compound with two or more epoxy groups in the presence of phosphorous and/or antimony catalyst, wherein the molar ratio of the isocyanate groups of the polyisocyanate compound to the epoxy groups of the polyepoxide compound is larger than 2:1 and less than 25:1, and wherein the process is conducted in the absence of a solvent with a boiling point higher than 200 °C, at 1 bar (absolute). The invention is also related to the resulting isocyanate-group terminated polyoxazolidinone compositions and a process for producing an isocyanate-group terminated polyoxazolidinone by removal of a solvent and/or unreacted polyisocyanate compound.. |