assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_35c163b846f1e43382aeed8dd7bad2a8 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-5313 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-527 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2377-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-265 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-042 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G69-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-5313 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-527 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-02 |
filingDate | 2022-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_66cbe262bcb562f4e5ce460634846aef http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b06d8f4c798cced9922c99e396312aa5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e0558842da6d35f91d2ad8d63bc4d1b5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2158fea8c180c2ee39c8a5b9652d436b |
publicationDate | 2022-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2022214755-A1 |
titleOfInvention | Flame retardant polyamide compositions, uses of same and processes for the preparation thereof |
abstract | The invention relates to a composition for a thermoplastic composite material, comprising: (a) from 65 to 95% by weight of at least one reactive semi-crystalline polyamide prepolymer having an average molar mass Mn of less than 5000 g/mol and having a volume median diameter Dv50 of the reactive semi-crystalline polyamide prepolymer powder particles of 10 to 300 μm; (b) from 5 to 35% by weight of at least one flame retardant selected from an at least partially meltable flame retardant in powder form and having a volume median diameter Dv50 of 10 to 300 μm, and a non-meltable flame retardant in the form of a pre-milled powder and having a volume median diameter Dv50 of 1 to 50 μm; and (c) from 0 to 2% by weight of at least one additive, and said reactive polyamide prepolymer comprising or consisting of at least one Z/BACT/XT copolyamide wherein: - BACT is an amide unit having a molar ratio of 10 to 65%; - XT is an amide unit having a molar ratio of 30 to 60 mol%; - Z Is an amide unit unit present at a molar ratio ranging from 5 to 30%; and wherein the molar sum Z + BACT + XT is equal to 100%, the sum of the constituents (a) + (b) + (c) is equal to 100%, and said reactive semi-crystalline polyamide prepolymer has a melting point Tf < 300°C, a glass transition temperature Tg > 80°C, and a difference between the melting point and the crystallization temperature Tf -Tc < 70°C. |