http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022203201-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3164a963ca21cec1151213cb1bb95e77 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-755 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-75 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-755 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-75 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25B1-04 |
filingDate | 2022-02-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8c0e90ee443ba90c365a537782746103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_056cea831db5092768c669e4a18d567d |
publicationDate | 2022-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2022203201-A1 |
titleOfInvention | Method for manufacturing core-shell structure by using rapid delithiation, core-shell structure manufactured thereby, and catalyst using same |
abstract | The present invention relates to a method for manufacturing a core-shell structure by using rapid delithiation, a core-shell structure manufactured thereby, and a catalyst using same. According to the present invention, a structure having a core with high electric conductivity and a shell having excellent reactivity can be manufactured by controlling crystallinity of an inner portion and a surface portion of a material through lithiation or delithiation. In addition, the changes in crystallinity and chemical characteristics of the material can be maximized through rapid delithiation. Therefore, the core-shell structure of the present invention has excellent conductivity and reactivity and can be effectively used as a water-splitting catalyst. In the present invention, lithiation and delithiation are employed only once without using an expensive material, such as a precious metal, and thus a core-shell structure with excellent catalytic characteristics can be manufactured by an economical and simple process. |