http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022200184-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_74b2654f32cbf5a0ebd14a6f91ddf54c |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2-006 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-1216 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C16-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C16-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C16-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C16-4412 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C16-442 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C16-4417 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C16-45525 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J2-00 |
filingDate | 2022-03-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1d1ac97d852c6ef84b9ce9d1f10d9aa6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6bce7890b084811c168a9f4802e59fca http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3073d0b22c21a965fd4f1963914eb92d |
publicationDate | 2022-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2022200184-A1 |
titleOfInvention | Particle coating by atomic layer deposition |
abstract | The present invention relates to a method for producing coated particles by atomic layer deposition, comprising the steps of: a) dispersing particles having reactive groups on their surface in an organic solvent, b) adding a first reactant in excess to the reactive groups on the surface, c) mixing the dispersion to react the first reactant with reactive groups on the surface of the particles, d) removing the excess of the first reactant by vacuum or by distillation or by azeotropic distillation, e) adding a second reactant in excess to the reactive groups on the surface obtained in step d), f) mixing the dispersion to react the second reactant with the first reactant on the surface of the particles, g) removing the excess of the second reactant by vacuum or by distillation or by azeotropic distillation. The organic solvent has a boiling point that is both at least 10°C higher than the boiling point of the first reactant and at least 10°C higher than the boiling point of the second reactant thus allowing the removal of the excess of the first reactant and the second reactant by vacuum or by distillation or by azeotropic distillation. |