abstract |
A thermoplastic resin composition of the present invention comprises: a polycarbonate resin; a polyester resin; rectangular cross-section glass fibers having a cross-sectional aspect ratio of about 1.5 to about 10, a cross-sectional minor diameter of about 2 to about 10 μm, and a length of about 1 to about 30 mm before processing; talc having an average particle size (D50) of about 7 to about 30 μm; and a phosphazene-based flame retardant, wherein the weight ratio of the glass fibers and the talc is about 1.5:1 to about 6:1. The thermoplastic resin composition is excellent in dimensional stability, flame retardancy, impact resistance, color, and the like. |