http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021092831-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_513ad31a4308c6fb6ee7b963b7e9bd19 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J31-32 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J31-32 |
filingDate | 2019-11-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f99d0711aed48961846231f0a4ec595c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_14fe3b35502985b383cb7dded07e48cf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_25b1ac5756445fb147f4c824dbd65050 |
publicationDate | 2021-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2021092831-A1 |
titleOfInvention | Method for preparing scr denitration catalyst |
abstract | A method for preparing a SCR denitration catalyst, specifically comprising the following steps: (1) weighing an appropriate amount of self-made or existing MOF nanoparticles; (2) preparing an Si-MOF support; (3) and taking the Si-MOF support obtained above, dispersing same in deionized water, adding an appropriate amount of water-soluble polymer thereto, and after same has dissolved completely, adding a potassium permanganate solution, adding potassium permanganate drop by drop and stirring to obtain a SCR denitration catalyst. The described method is able to prepare a porous spherical structure SCR denitration catalyst that has a large specific surface area and a good catalytic performance. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113769785-A |
priorityDate | 2019-11-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 37.