abstract |
The present invention provides a tire which exhibits excellent long-lasting performance . The present invention pertains to a tire which has a tread comprising a rubber composition which satisfies formulas (1)-(3) within 180 days after vulcanization. (1): Hso/Hsa×100≥95, wherein Hso is curing at a normal temperature and Hsa is curing at a normal temperature after heat-treating at 80°C for 168 hours. (2): As/Ts×100≤70, wherein Ts is sulfur content before extracting acetone and As is sulfur content after extracting acetone. (3): Swell≤330, wherein Swell is toluene swelling index. |