abstract |
A method of producing a carbonated composite material is described that includes: providing a carbonatable cementitious material in particulate form; mixing the carbonatable cementitious material with water to produce a mix; forming a predetermined shape with the mix, wherein the predetermined shape has an initial pore stmcture containing an initial pore solution having a first pH; pre-conditioning the predetermined shape to remove a predetermined amount of the water from the predetermined shape to produce a pre-Δ conditioned shape; carbonating the pre-conditioned shape in an environment comprising carbon dioxide to produce a modified pore stmcture containing a modified pore solution having and a second pH, wherein the difference between the first pH and the second pH is represented by a ΔpH, and the ΔpH is 1.0 or less, 0.75 or less, 0.5 or less, 0.25 or less, or about 0.0. A calcium silicate composition including solid components and liquid components having improved pore solution pH stability is also disclosed. |