http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021068737-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0ee33b0e3e7398cf6fc957eeee59d510 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F9-08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F9-08 |
filingDate | 2020-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_13bdc50494cc77726845dbd0966c86be http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1fae7415b50eb5dbbb6a878b095229b1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_51fe4ea3b49561712c5c46ba7097196b |
publicationDate | 2021-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2021068737-A1 |
titleOfInvention | Flexible mullite fiber aerogel material and preparation method thereof |
abstract | Provided is a flexible mullite fiber aerogel material and a preparation method thereof. The method of preparing the flexible mullite fiber aerogel material comprises mixing a polymer material with a solvent to obtain a polymer solution; mixing the polymer solution with a mullite precursor and a catalyst to obtain a spinning precursor solution; performing a solution blow spinning treatment on the spinning precursor solution to obtain a composite fiber aerogel material containing the polymer material, the mullite precursor and the catalyst; and heating the composite fiber aerogel material to obtain the flexible mullite fiber aerogel material. |