abstract |
A thermoplastic resin composition of the present invention comprises: about 100 parts by weight of a polycarbonate resin; about 10 to about 40 parts by weight of a polyester resin; about 0.1 to about 1.0 parts by weight of a chain extender; about 50 to about 80 parts by weight of glass fibers; about 10 to about 25 parts by weight of a phosphorus flame retardant; and about 1 to about 7 parts by weight of a modified polyolefin, wherein the weight ratio of the polyester resin and the chain extender is about 1:0.01 to about 1:0.06. The thermoplastic resin composition is excellent in dimensional stability, flame retardancy, impact resistance, and the like. |