abstract |
The present invention relates to a mixer system for producing aqueous coating materials from at least one aqueous pigment paste A, comprising at least one effect pigment, and at least one pigment-free component B, comprising an aqueous, acrylate-based microgel dispersion having a glass transition temperature Tg of 50 to 60°C, where both the aqueous pigment paste A and the component B each have a VOC value of less than or equal to 250 g/L. The present invention further relates to a method for producing aqueous coating materials having a VOC content of 0 to 250 g/L, more particularly of 100 to 250 g/L, in which the individual components A and B are stored separately and not mixed until shortly before application, to give the aqueous coating material. The present invention lastly relates to the use of a mixer system of the invention for producing aqueous coating materials for refinishing and/or for the coating of automobile bodies and/or plastics parts. |