http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020262006-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-7242 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D65-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B38-145 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 |
filingDate | 2020-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_343f29713ab107142e50cbd7571d3ba5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0beb2a07bae2aa9643dc069be120b2de http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f09196e4668c5d39b171791cfb21a350 |
publicationDate | 2020-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2020262006-A1 |
titleOfInvention | Gas barrier laminate and packaging material |
abstract | The present invention provides: a laminate in which a good gas barrier property is maintained even though a printing layer and a bonding layer formed with an adhesive having a gas barrier property are arranged adjacent to each other; and a packaging material obtained with the laminate. A laminate according to the present invention is characterized by including: a base material; a sealant layer; a printing layer disposed between the base material and the sealant layer and formed with a liquid ink; and a bonding layer disposed between the printing layer and the sealant layer so as to be in contact with the printing layer, the bonding layer being formed with an adhesive that satisfies at least one of the condition that the oxygen barrier property of a coating film applied at 3 g/m2 (solid content), at 23ÂșC and 0%RH, is less than or equal to 300 cc/m2/day/atm and the condition that the water vapor barrier property thereof is less than or equal to 120 g/m2/day, wherein the application amount of the liquid ink (solid content), except for colorant, contained in the printing layer is less than or equal to 1.1 g/m2. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022138188-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7207617-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022220151-A1 |
priorityDate | 2019-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 303.