http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020241672-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_696ca0ae93d5cf5a686273601361781f |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-03 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 2020-05-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0a72d1644971debdc6f77c1c7d4e4d42 |
publicationDate | 2020-12-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2020241672-A1 |
titleOfInvention | Composition, film and method for producing film |
abstract | Provided are: a composition capable of providing a transparent film which exhibits high sliding properties and heat resistance and in which turbidity is suppressed; a film formed from the composition; and a method for producing the film. This composition contains: 25-70 parts by mass of a bisphenol A type polycarbonate (A) having a weight average molecular weight of 20,000-35,000; 26.5-71.5 parts by mass of an aromatic polycarbonate (B) other than the bisphenol A type polycarbonate (A), which has a glass transition temperature of 160°C or higher when measured using a differential scanning calorimeter; and 3.5-7.5 parts by mass of a polyarylate (C) having a weight average molecular weight of 45,000-80,000. |
priorityDate | 2019-05-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |