Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-022 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2077-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2377-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2423-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2423-16 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16L11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-265 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-26 |
filingDate |
2020-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_68dcffcef3d45dec6daca8734294b4ae |
publicationDate |
2020-09-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2020175290-A1 |
titleOfInvention |
Tube, and polyamide resin composition |
abstract |
Provided is a tube comprising a layer containing: 60-80 mass% of a semi-aromatic polyamide; and 15-40 mass% of an elastomer modified with an unsaturated compound having at least one selected from among a carboxyl group and an acid anhydride group, wherein the layer has a phase-separated structure including a phase (A) containing the semi-aromatic polyamide and a phase (B) containing the elastomer, the phase (A) being a continuous phase, and the phase (B) being a dispersion phase dispersed in the phase (A), and in a cross-sectional image of the layer as observed by an electron microscope, the average number of the phase (B) having a major axis diameter of at least 2 μm and existing per 100 square μm, is at most 1/100 μm2. Also provided is a polyamide resin composition obtained by melt-kneading a semi-aromatic polyamide and an elastomer modified with an unsaturated compound having at least one selected from among a carboxyl group and an acid anhydride group, wherein the total concentration of the carboxyl group and the acid anhydride group in 1 g of the elastomer is 85-250 μeq/g. |