Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5521cb08df898c00aa9c92a3d1b371d3 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2327-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2325-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2377-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2369-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2375-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2367-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D189-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D65-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D65-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D65-466 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-20 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-06 |
filingDate |
2019-10-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1666c9189eed7a845650d4d99f406586 |
publicationDate |
2020-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2020084632-A1 |
titleOfInvention |
A biodegradable polymeric substrate and a method of producing the substrate |
abstract |
The present invention discloses a method of making a non-biodegradable flexible packaging substrate biodegradable. The method comprises the steps of (i) providing a substrate web from an unwind to a coating station (402), (ii) applying thin layer of uniform deposition of a curable coating on atleast one surface of the substrate partially or completely by the coating station wherein the external surface of the substrate is essentially coated, (iii) curing the coating applied on the substrate web by a curing unit, and (iv) collecting the coated substrate web in roll at rewind. Further, the thickness of the thin layer of uniform deposition is in the range of 0.01gsm to 10gsm. Representative drawing |