Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-265 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-26 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00 |
filingDate |
2019-09-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9af5ea463ea1637a47e55a2a6e071e3c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_73e55ff254f5af31e9cc4c2dd371c641 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_59bd3f6c2815333ba00851184ec37a78 |
publicationDate |
2020-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2020050326-A1 |
titleOfInvention |
Thermoplastic resin composition |
abstract |
A thermoplastic resin composition which contains 3-10 parts by mass of (B) a modified polyolefin that has a melt flow rate (MFR) of 0.1-0.6 g/10 minutes at a temperature of 240°C under a load of 2.16 kg per 100 parts by mass of (A) a thermoplastic resin that has a melting point of 270°C or more. It is preferable that the modified polyolefin (B) has a 1% decomposition temperature of 300-450°C; and it is also preferable that the thermoplastic resin (A) is a polyamide resin. |
priorityDate |
2018-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |