Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_95585944cd76ddfb6dc33ed2a0b84403 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-162 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T442-20 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L91-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J123-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J191-06 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J191-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B5-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J123-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J123-10 |
filingDate |
2019-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cf1fb783c06e37f152d6134099792c24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b4b92dbf068dcd139c6bacfc632dd34f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ab7fec74c31e1c01a74101820fbcb387 |
publicationDate |
2020-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2020027222-A1 |
titleOfInvention |
Polypropylene-based adhesive and method for producing same |
abstract |
Provided is a polypropylene-based adhesive which contains a polypropylene-based resin (A') which is obtained by reducing the weight average molecular weight of a polypropylene-based resin (A) by decomposition. The polypropylene-based resin (A) has a latent heat of fusion (ΔH-D) of 0-80 J/g, as obtained from a melting endotherm curve obtained by holding a sample at a temperature of -10°C in a nitrogen atmosphere for 5 minutes and then increasing the temperature at a rate of 10ºC/min using a differential scanning calorimeter (DSC). |