abstract |
The present invention relates to an olefin-based polymer having (1) a density of 0.85 to 0.865 g/cc, (2) a melt index (MI) of 0.1 g/10 min. to 3.0 g/10 min. at 190℃ under a load condition of 2.16 kg, (3) a soluble fraction (SF) of 10% or more at -20℃ in cross-fractionation chromatography (CFC), and a weight average molecular weight (MW) for corresponding fraction of 50,000 g/mol to 500,000 g/mol. The olefin-based polymer according to the present invention exhibits improved anti-blocking properties as a low-density olefin-based polymer. |