http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019083211-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33c922e05f6133b7d72dbb849d77487d |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F20-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-06 |
filingDate | 2018-10-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_41dced400e116c6f2625e9953356ce42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c21334a9751f288e083fd847ecdd3fb0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3422650422128f184c9d732c0b27645b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2947757dc4a91bfdbe160de0f167a57c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_36ae66d6dc42db3e595d8becdc5bf162 |
publicationDate | 2019-05-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2019083211-A1 |
titleOfInvention | PROCESS FOR THE PREPARATION OF SUPERABSORBENT POLYMER |
abstract | The present invention provides a method for producing a superabsorbent resin which enables production of a superabsorbent resin capable of exhibiting an excellent absorption rate including a uniform porous structure through a simple and economical process. The method for producing a superabsorbent resin includes crosslinking a water-soluble ethylenically unsaturated monomer having at least partially neutralized acid groups in the presence of an internal crosslinking agent to form a hydrogel polymer comprising a first crosslinked polymer; Drying and pulverizing the hydrogel polymer; The pulverized polymer is classified into polymer particles having a particle diameter of at least 10 to 150 mu m , polymer particles having a particle diameter of 150 to 200 mu m , and polymer particles having a particle diameter of 200 to 850 mu m to obtain a base resin powder ; And cross-linking the base resin powder. In the cross-linking polymerization step, the foaming polymerization is carried out in the presence of polymer particles having an average particle diameter of 10 to 200 μm and an anionic surfactant obtained in the classification step. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113811337-A |
priorityDate | 2017-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 87.