abstract |
The infrared stealth coating and the preparation method thereof, the infrared stealth coating comprises: 40.0-50.0% silicone resin, 1.0-40.0% filler, 10.0-20.0% pigment, 0.5-5.0% dispersant, by weight percentage 0.2 to 1.5% wetting agent, 0.5 to 5.0% thickener, 0.0 to 1.5% leveling agent, 0.5 to 3.0% of filming aid, 0.0 to 0.5% of defoamer and balance Deionized water. |