Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5f7f120efe096284c7389702c969cf3d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2201-026 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2309-04 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-228 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-30 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-228 |
filingDate |
2018-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_82995fade8733716be6d2906902942fd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eeae7e071f6e6eebde2a8ba4dfbec1b6 |
publicationDate |
2019-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2019017240-A1 |
titleOfInvention |
PROCESS FOR PRODUCING RUBBER FOAM |
abstract |
A method for producing a foam rubber by foaming a polymer latex, wherein the polymer latex has a solid content concentration of 60.0% by weight or more and 100 parts by weight of the polymer in the polymer latex. Method of producing a foam rubber using an agent having a content ratio of 0.001 to 1.0 parts by weight and a viscosity at a temperature of 25.degree. C. of 370 cps or less when the solid content concentration is adjusted to 66.0% by weight I will provide a. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019183119-A |
priorityDate |
2017-07-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |