Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6d9b63f4b9addf71f8c5674c4d94290a |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2004-027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2004-021 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-386 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-587 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-133 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-134 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-583 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-0471 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-364 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-625 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-362 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-366 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1395 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1393 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-38 |
filingDate |
2017-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f20b1ad38b17f146395756378265762 |
publicationDate |
2018-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2018198282-A1 |
titleOfInvention |
Carbon-silicon composite material, negative electrode and secondary battery |
abstract |
A carbon-silicon composite material which is suitable as a battery negative electrode material. This carbon-silicon composite material is configured such that silicon particles are present in a thermolysis product of a resin; and if this carbon-silicon composite material is immersed in an electrolyte solution ((ethylene carbonate)/(diethyl carbonate) at the volume ratio of 1/1) under the conditions of 760 mmHg, 30°C and 60 min, the absorption amount of the electrolyte solution per 1 g of this carbon-silicon composite material is 0.65-1.5 mL. |