Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6e310a5294181f80021bee242e5682dc http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8e0bf0928b608797b70bbc2b91c7e52e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2250-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2250-24 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-244 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4063 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4238 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-698 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-69 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-7671 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6208 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-69 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-24 |
filingDate |
2018-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_df0602a868e012844af7620cad0832a0 |
publicationDate |
2018-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2018191459-A1 |
titleOfInvention |
Thermoplastic polyurethane and composite article |
abstract |
A thermoplastic polyurethane is the reaction product of a polybutadiene diol, a polyester diol, and a isocyanate component. The polybutadiene diol has a weight average molecular weight (Mw) of from 200 to 20,000 g/mol. The polyester diol has a melting point of from 40 to 90°C. The reactants allow the thennoplastic polyurethane itself to have a melt flow index measured at 120°C and 22.6 kg of from 0.1 to 200 grams, per 10 minutes as measured according to ASTM 1238. The thermoplastic polyurethane also has a melting point of from 50 to 300°C. The thermoplastic polyurethane is used to form a composite article. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3653658-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020099624-A1 |
priorityDate |
2017-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |