abstract |
In some embodiments, the present disclosure provides a composition comprising from 5 phr to 30 phr of a PEDM terpolymer having 1 to 10 wt% diene, 13 to 40 wt% ethylene, and 15 to 85 wt% propylene, based on the weight of the PEDM terpolymer. The composition further comprises from 70 phr to 95 phr of an ethylene-based copolymer comprising an ethylene content different than the first polymer, a C3 to C 12 α-olefin, and, optionally, one or more dienes. |