abstract |
An example inkjet primer fluid includes an alkoxysilane, a surfactant, a co-solvent, and a balance of water; and is at least substantially colorless. In an example method, a primer fluid, including an alkoxysilane, a surfactant, a co-solvent, and a balance of water, is thermal inkjet printed from a thermal inkjet printhead to form a silicon dioxide film on a resistor. Then, a jettable composition, including suspended nanoparticles, is thermal inkjet printed from the thermal inkjet printhead. In another example method, suspended nanoparticles, an alkoxysilane, and a growth mediator are combined to form a mixture. The mixture is heated to a temperature ranging from about 60°C to about 80°C and stirred for about 12 hours to about 36 hours to form silicon dioxide coated, suspended nanoparticles. Then, a surfactant, a zwitterionic stabilizer, a co-solvent, and a balance of water are added to the mixture to form a stabilized, jettable composition. |